Abstract: Purpose
This specification covers the requirements for silver deposited on metal parts with a copper strike between the basis metal and the silver deposit.
Application
This process has been used typically to provide a bearing surface and to prevent galling or seizing of metal surfaces of parts made of materials where a high baking temperature may be detrimental to the properties of the basis material.
Safety-Hazardous Materials
While the materials, methods, applications, and processes described or referenced in this specification may involve the use of hazardous materials, this specification does not address the hazards which may be involved in such use. It is the sole responsibility of the user to ensure familiarity with the safe and proper use of any hazardous materials and to take necessary precautionary measures to ensure the health and safety of all personnel involved.
This specification covers the requirements for silver deposited on metal parts with a copper strike between the basis metal and the silver deposit.
Application
This process has been used typically to provide a bearing surface and to prevent galling or seizing of metal surfaces of parts made of materials where a high baking temperature may be detrimental to the properties of the basis material.
Safety-Hazardous Materials
While the materials, methods, applications, and processes described or referenced in this specification may involve the use of hazardous materials, this specification does not address the hazards which may be involved in such use. It is the sole responsibility of the user to ensure familiarity with the safe and proper use of any hazardous materials and to take necessary precautionary measures to ensure the health and safety of all personnel involved.
Collections
:
Show full item record
contributor author | SAE - SAE International | |
date accessioned | 2017-09-04T16:46:07Z | |
date available | 2017-09-04T16:46:07Z | |
date copyright | 2015.01.01 | |
date issued | 2015 | |
identifier other | WBLUJFAAAAAAAAAA.pdf | |
identifier uri | http://yse.yabesh.ir/std/handle/yse/109409 | |
description abstract | Purpose This specification covers the requirements for silver deposited on metal parts with a copper strike between the basis metal and the silver deposit. Application This process has been used typically to provide a bearing surface and to prevent galling or seizing of metal surfaces of parts made of materials where a high baking temperature may be detrimental to the properties of the basis material. Safety-Hazardous Materials While the materials, methods, applications, and processes described or referenced in this specification may involve the use of hazardous materials, this specification does not address the hazards which may be involved in such use. It is the sole responsibility of the user to ensure familiarity with the safe and proper use of any hazardous materials and to take necessary precautionary measures to ensure the health and safety of all personnel involved. | |
language | English | |
title | SAE AMS2412K | num |
title | (R) Plating, Silver Copper Strike, Low Bake | en |
type | standard | |
page | 8 | |
status | Active | |
tree | SAE - SAE International:;2015 | |
contenttype | fulltext |