• 0
    • ارسال درخواست
    • حذف همه
    • Industrial Standards
    • Defence Standards
  • درباره ما
  • درخواست موردی
  • فهرست استانداردها
    • Industrial Standards
    • Defence Standards
  • راهنما
  • Login
  • لیست خرید شما 0
    • ارسال درخواست
    • حذف همه
View Item 
  •   YSE
  • Industrial Standards
  • TAPPI - TAPPI
  • View Item
  •   YSE
  • Industrial Standards
  • TAPPI - TAPPI
  • View Item
  • All Fields
  • Title(or Doc Num)
  • Organization
  • Year
  • Subject
Advanced Search
JavaScript is disabled for your browser. Some features of this site may not work without it.

Archive

TAPPI T 226 CM

Specific external surface of pulp

Organization:
TAPPI - TAPPI
Year: 2011

Abstract: This method, based on the silvering method devised by Clark (1), is used to determine the specific exposed surface of unbeaten, or only slightly beaten, chemical pulps, groundwood, wood flour, and similar materials. It is not suitable for finely fibrillated or well-beaten fibers, since the silvering step causes some of the finest fibrils to collapse and hence lowers the exposed area (2).
URI: http://yse.yabesh.ir/std;jsein=autho1:%22NAVY%20-%20YD%20-%20Naval%20Facilities%114ngineering%20Command%22/handle/yse/59033
Subject: Beater
Collections :
  • TAPPI - TAPPI
  • Download PDF : (127.7Kb)
  • Show Full MetaData Hide Full MetaData
  • Statistics

    TAPPI T 226 CM

Show full item record

contributor authorTAPPI - TAPPI
date accessioned2017-09-04T15:55:42Z
date available2017-09-04T15:55:42Z
date copyright2011.01.01
date issued2011
identifier otherQVSSKEAAAAAAAAAA.pdf
identifier urihttp://yse.yabesh.ir/std;jsein=autho1:%22NAVY%20-%20YD%20-%20Naval%20Facilities%114ngineering%20Command%22/handle/yse/59033
description abstractThis method, based on the silvering method devised by Clark (1), is used to determine the specific exposed surface of unbeaten, or only slightly beaten, chemical pulps, groundwood, wood flour, and similar materials. It is not suitable for finely fibrillated or well-beaten fibers, since the silvering step causes some of the finest fibrils to collapse and hence lowers the exposed area (2).
languageEnglish
titleTAPPI T 226 CMnum
titleSpecific external surface of pulpen
typestandard
page7
statusActive
treeTAPPI - TAPPI:;2011
contenttypefulltext
subject keywordsBeater
subject keywordsFineness
subject keywordsGroundwood
subject keywordsPulp
subject keywordsSpecific surface
subject keywordsWood flour
DSpace software copyright © 2017-2020  DuraSpace
نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
yabeshDSpacePersian
 
DSpace software copyright © 2017-2020  DuraSpace
نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
yabeshDSpacePersian