• 0
    • ارسال درخواست
    • حذف همه
    • Industrial Standards
    • Defence Standards
  • درباره ما
  • درخواست موردی
  • فهرست استانداردها
    • Industrial Standards
    • Defence Standards
  • راهنما
  • Login
  • لیست خرید شما 0
    • ارسال درخواست
    • حذف همه
View Item 
  •   YSE
  • Industrial Standards
  • TAPPI - TAPPI
  • View Item
  •   YSE
  • Industrial Standards
  • TAPPI - TAPPI
  • View Item
  • All Fields
  • Title(or Doc Num)
  • Organization
  • Year
  • Subject
Advanced Search
JavaScript is disabled for your browser. Some features of this site may not work without it.

Archive

TAPPI T 254 CM

Cupriethylenediamine disperse viscosity of pulp (falling ball method)

Organization:
TAPPI - TAPPI
Year: 2010

Abstract: This method describes a rapid procedure (1, 2, 3) for the measurement of the viscosity of 1% cellulose solutions using cupriethylenediamine saturated with cupric hydroxide [Cu(OH)2] as the solvent. For convenience, this may be referred to as Cu(En)2 or CED.
This method is the preferred procedure for pulps containing more than 4% lignin; however, many high yield pulps, at levels above 50%, contain sufficient lignin (in excess of 10%) to interfere with the test. The falling ball method may be used over the entire range of bleached and unbleached pulps and is well suited to production control. However, the preferred procedure for pulps with less than 4% lignin, as defined by TAPPI T 222 "Acid-Insoluble Lignin in Wood and Pulp," is TAPPI T 230 "Viscosity of Pulp (Capillary Viscometer Method)," which should be used for referee purposes on these pulps.
This procedure covers preparation of cupriethylenediamine, dissolving the sample, viscometer calibration, and measurement of the viscosity of the sample solution.
URI: http://yse.yabesh.ir/std;jsery=auth=177/handle/yse/10434
Subject: Cellulose
Collections :
  • TAPPI - TAPPI
  • Download PDF : (188.9Kb)
  • Show Full MetaData Hide Full MetaData
  • Statistics

    TAPPI T 254 CM

Show full item record

contributor authorTAPPI - TAPPI
date accessioned2017-09-04T15:12:01Z
date available2017-09-04T15:12:01Z
date copyright2010.01.01
date issued2010
identifier otherAQKIRCAAAAAAAAAA.pdf
identifier urihttp://yse.yabesh.ir/std;jsery=auth=177/handle/yse/10434
description abstractThis method describes a rapid procedure (1, 2, 3) for the measurement of the viscosity of 1% cellulose solutions using cupriethylenediamine saturated with cupric hydroxide [Cu(OH)2] as the solvent. For convenience, this may be referred to as Cu(En)2 or CED.
This method is the preferred procedure for pulps containing more than 4% lignin; however, many high yield pulps, at levels above 50%, contain sufficient lignin (in excess of 10%) to interfere with the test. The falling ball method may be used over the entire range of bleached and unbleached pulps and is well suited to production control. However, the preferred procedure for pulps with less than 4% lignin, as defined by TAPPI T 222 "Acid-Insoluble Lignin in Wood and Pulp," is TAPPI T 230 "Viscosity of Pulp (Capillary Viscometer Method)," which should be used for referee purposes on these pulps.
This procedure covers preparation of cupriethylenediamine, dissolving the sample, viscometer calibration, and measurement of the viscosity of the sample solution.
languageEnglish
titleTAPPI T 254 CMnum
titleCupriethylenediamine disperse viscosity of pulp (falling ball method)en
typestandard
page10
statusActive
treeTAPPI - TAPPI:;2010
contenttypefulltext
subject keywordsCellulose
subject keywordsCuene
subject keywordsPulp
subject keywordsViscosity
DSpace software copyright © 2017-2020  DuraSpace
نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
yabeshDSpacePersian
 
DSpace software copyright © 2017-2020  DuraSpace
نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
yabeshDSpacePersian