TAPPI - TAPPI: Recent submissions
Now showing items 241-260 of 533
-
-
TAPPI TIP 0304-07
Abstract: Why cross direction warp in corrugated board occurs and how to correct it.Subject(s) : Corrugated boards , Cross direction , Moisture control , Warpage , -
TAPPI T 1211 SP
Abstract: This standard practice establishes the "self certification" procedures for an organization to nominate itself, and be accepted, as a TAPPI calibration laboratory for inclusion in the listing of such sources within the ...Subject(s) : Calibration , Instrument characteristics , Laboratories , Measuring instruments , Standard practice , Standards , -
TAPPI UM 23
Abstract: This method is used to determine the weight on a moisture-free basis per unit volume of wet wood chips, the bulk density. For purposes of reference, a standard pressure of 11 kPa (225 lb/ft2) has been chosen. ...Subject(s) : Bulk density , Chips , Density , -
TAPPI T 406 OM
Abstract: This method describes two procedures for the determination of reducible sulfur in paper and paperboard within the context of the given definitions.
The quantitative procedure found in Section 9 gives a measure of the ... -
TAPPI T 545 OM
Abstract: This method describes a procedure which can be applied to determine the variation in mass per unit area in the cross-machine direction, commonly referred to as the grammage (or basis weight) profile. This method is appropriate ...Subject(s) : Basis weight , Cross direction , Profiles , Variations , -
TAPPI TIP 0402-27
Abstract: This Technical Information Paper (TIP) provides guidelines for inspecting digester vessels in alkaline pulping service. (The term ‘digester vessels' refers to continuous digesters or impregnation vessels in ...Subject(s) : continuous digesters , Corrosion , cracks , digesters , impregnation , inspection , nondestructive tests , stress corrosion , welds , -
TAPPI TIP 0404-57
Abstract: Poor cross-machine direction (CD) moisture profiles result in non-uniform paper end-use properties, converting problems, and poor runnability in the form of wrinkles and breaks. Fiber costs (such as heavy edges) and energy ...Subject(s) : Cross direction , Dryer pockets , Dryers , Felts , Forming sections , Humidity , Infrared detectors , Measurement , Moisture content , Moisture control , Nip , Profiles , Temperature , Thermography , Water permeability , -
TAPPI T 821 OM
Abstract: This method is used to measure the force required to separate corrugated board between the flute tips of corrugated medium and its linerboard facings.