• 0
    • ارسال درخواست
    • حذف همه
    • Industrial Standards
    • Defence Standards
  • درباره ما
  • درخواست موردی
  • فهرست استانداردها
    • Industrial Standards
    • Defence Standards
  • راهنما
  • Login
  • لیست خرید شما 0
    • ارسال درخواست
    • حذف همه
View Item 
  •   YSE
  • Industrial Standards
  • TAPPI - TAPPI
  • View Item
  •   YSE
  • Industrial Standards
  • TAPPI - TAPPI
  • View Item
  • All Fields
  • Title(or Doc Num)
  • Organization
  • Year
  • Subject
Advanced Search
JavaScript is disabled for your browser. Some features of this site may not work without it.

Archive

TAPPI T 807 OM

Bursting strength of linerboard

Organization:
TAPPI - TAPPI
Year: 2011

Abstract: Scope and summary
This method describes a procedure for measuring the bursting strength of linerboard using a disk shaped diaphragm. Basis weights for this method should be 98 g/m2 (20#/MSF) and higher. The minimum burst should be 350 kPa (51 psi). This method may also be used to test paperboard.
A specimen is clamped between two platens with circular openings in their centers. An expansible diaphragm is distended through the lower platen by means of hydraulic pressure until the specimen ruptures. The maximum hydraulic pressure when the specimen ruptures is recorded.
For the bursting strength of paper with basis weights below 98 g/m2, use TAPPI T 403 "Bursting Strength of Paper." For corrugated combined board, see TAPPI T 810 "Bursting Strength of Corrugated Board."
URI: http://yse.yabesh.ir/std;jsessionid=47037D83FCDCAC426159DD6E273C9FCD/handle/yse/223218
Subject: Burst strength
Collections :
  • TAPPI - TAPPI
  • Download PDF : (120.4Kb)
  • Show Full MetaData Hide Full MetaData
  • Statistics

    TAPPI T 807 OM

Show full item record

contributor authorTAPPI - TAPPI
date accessioned2017-09-04T18:41:44Z
date available2017-09-04T18:41:44Z
date copyright2011.01.01
date issued2011
identifier otherJXSSKEAAAAAAAAAA.pdf
identifier urihttp://yse.yabesh.ir/std;jsessionid=47037D83FCDCAC426159DD6E273C9FCD/handle/yse/223218
description abstractScope and summary
This method describes a procedure for measuring the bursting strength of linerboard using a disk shaped diaphragm. Basis weights for this method should be 98 g/m2 (20#/MSF) and higher. The minimum burst should be 350 kPa (51 psi). This method may also be used to test paperboard.
A specimen is clamped between two platens with circular openings in their centers. An expansible diaphragm is distended through the lower platen by means of hydraulic pressure until the specimen ruptures. The maximum hydraulic pressure when the specimen ruptures is recorded.
For the bursting strength of paper with basis weights below 98 g/m2, use TAPPI T 403 "Bursting Strength of Paper." For corrugated combined board, see TAPPI T 810 "Bursting Strength of Corrugated Board."
languageEnglish
titleTAPPI T 807 OMnum
titleBursting strength of linerboarden
typestandard
page6
statusActive
treeTAPPI - TAPPI:;2011
contenttypefulltext
subject keywordsBurst strength
subject keywordsLinerboards
DSpace software copyright © 2017-2020  DuraSpace
نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
yabeshDSpacePersian
 
DSpace software copyright © 2017-2020  DuraSpace
نرم افزار کتابخانه دیجیتال "دی اسپیس" فارسی شده توسط یابش برای کتابخانه های ایرانی | تماس با یابش
yabeshDSpacePersian