description abstractScope: This test method applies to hot-poured asphalt crack sealant used in the construction and maintenance of roadways as specified in MP 25 and PP 85. The test method is used to determine the extendibility and strain energy density (SED) of sealants at low temperature. It can be used with unaged material or with material aged according to T 367. The test apparatus is designed for testing within the temperature range from –4 to –40°C. This standard covers the determination of extendibility and percent modulus decay in hot-poured asphalt crack sealant with the use of direct tension testing and by applying the tensile stress–strain test.
languageEnglish
titleEnglish -- Standard Method of Test for Evaluation of the Low-Temperature Tensile Property of Hot-Poured Asphalt Crack Sealant by Direct Tension Testen
titleAASHTO T 369num
typestandard
page10
statusActive
treeAASHTO - American Association of State Highway and Transportation Officials:;2017
contenttypefulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record