TAPPI T 822 OM
Ring crush of paperboard (rigid support method)
Organization:
TAPPI - TAPPI
Year: 2011
Abstract: The ring crush test correlates with edgewise compression strength of paperboard (1,2).
This method is intended for paperboard between 0.28 mm (0.011 in.) and 0.61 mm (0.024 in.) thick. It may be used with less reliability for paperboard as thin as 0.18 mm (0.007 in.) and as thick as 0.76 mm (0.030 in.).
NOTE 1: Caution should be used when testing linerboard less or greater than the specified thickness as the results may be less reliable. For papers thinner than 0.28 mm (0.011 in.), test values may result from a combination of both buckling failure and pure compression. For papers thicker than specified, strain within the sample arising from bending the specimens into a cylinder may impact test results (3,4).
This method is intended for paperboard between 0.28 mm (0.011 in.) and 0.61 mm (0.024 in.) thick. It may be used with less reliability for paperboard as thin as 0.18 mm (0.007 in.) and as thick as 0.76 mm (0.030 in.).
NOTE 1: Caution should be used when testing linerboard less or greater than the specified thickness as the results may be less reliable. For papers thinner than 0.28 mm (0.011 in.), test values may result from a combination of both buckling failure and pure compression. For papers thicker than specified, strain within the sample arising from bending the specimens into a cylinder may impact test results (3,4).
Subject: Compression tests
Collections
:
Show full item record
| contributor author | TAPPI - TAPPI | |
| date accessioned | 2017-09-04T16:02:28Z | |
| date available | 2017-09-04T16:02:28Z | |
| date copyright | 01/01/2011 | |
| date issued | 2011 | |
| identifier other | RNTCOEAAAAAAAAAA.pdf | |
| identifier uri | http://yse.yabesh.ir/std;quessionid=4703-Sta081D206/handle/yse/65665 | |
| description abstract | The ring crush test correlates with edgewise compression strength of paperboard (1,2). This method is intended for paperboard between 0.28 mm (0.011 in.) and 0.61 mm (0.024 in.) thick. It may be used with less reliability for paperboard as thin as 0.18 mm (0.007 in.) and as thick as 0.76 mm (0.030 in.). NOTE 1: Caution should be used when testing linerboard less or greater than the specified thickness as the results may be less reliable. For papers thinner than 0.28 mm (0.011 in.), test values may result from a combination of both buckling failure and pure compression. For papers thicker than specified, strain within the sample arising from bending the specimens into a cylinder may impact test results (3,4). | |
| language | English | |
| title | TAPPI T 822 OM | num |
| title | Ring crush of paperboard (rigid support method) | en |
| type | standard | |
| page | 5 | |
| status | Active | |
| tree | TAPPI - TAPPI:;2011 | |
| contenttype | fulltext | |
| subject keywords | Compression tests | |
| subject keywords | Corrugated boards | |
| subject keywords | Edge crush resistance | |
| subject keywords | Fiberboards | |
| subject keywords | Paperboard | |
| subject keywords | Ring crush tests |