Show simple item record

Ring crush of paperboard (rigid support method)

contributor authorTAPPI - TAPPI
date accessioned2017-09-04T16:02:28Z
date available2017-09-04T16:02:28Z
date copyright01/01/2011
date issued2011
identifier otherRNTCOEAAAAAAAAAA.pdf
identifier urihttp://yse.yabesh.ir/std;quessionid=4703-Sta081D206/handle/yse/65665
description abstractThe ring crush test correlates with edgewise compression strength of paperboard (1,2).
This method is intended for paperboard between 0.28 mm (0.011 in.) and 0.61 mm (0.024 in.) thick. It may be used with less reliability for paperboard as thin as 0.18 mm (0.007 in.) and as thick as 0.76 mm (0.030 in.).
NOTE 1: Caution should be used when testing linerboard less or greater than the specified thickness as the results may be less reliable. For papers thinner than 0.28 mm (0.011 in.), test values may result from a combination of both buckling failure and pure compression. For papers thicker than specified, strain within the sample arising from bending the specimens into a cylinder may impact test results (3,4).
languageEnglish
titleTAPPI T 822 OMnum
titleRing crush of paperboard (rigid support method)en
typestandard
page5
statusActive
treeTAPPI - TAPPI:;2011
contenttypefulltext
subject keywordsCompression tests
subject keywordsCorrugated boards
subject keywordsEdge crush resistance
subject keywordsFiberboards
subject keywordsPaperboard
subject keywordsRing crush tests