Standard Method of Test for Evaluation of the Low-Temperature Tensile Property of Bituminous Sealants by Direct Tension Test

contributor authorAASHTO - American Association of State Highway and Transportation Officials
date accessioned2017-09-04T16:39:07Z
date available2017-09-04T16:39:07Z
date copyright01/01/2010 (R 2013)
date issued2013
identifier otherVKFBGFAAAAAAAAAA.pdf
identifier urihttps://yse.yabesh.ir/std/handle/yse/102741
description abstractThis test method applies to bituminous sealants used in the construction and maintenance of roadways.
The test method is used to determine the extensibility and strain energy density (SED) of sealants at low temperature. It can be used with unaged material or with material aged using TP 86. The test apparatus is designed for testing within the temperature range from –4° to –40°C.
This standard covers the determination of extensibility and percent modulus decay in bituminous sealants with the use of direct tension testing and by applying the tensile stress–strain test.
languageEnglish
titleAASHTO TP 88num
titleStandard Method of Test for Evaluation of the Low-Temperature Tensile Property of Bituminous Sealants by Direct Tension Testen
typestandard
page10
statusActive
treeAASHTO - American Association of State Highway and Transportation Officials:;2013
contenttypefulltext


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record