Standard Method of Test for Resistance of Compacted Asphalt Mixtures to Moisture-Induced Damage

contributor authorAASHTO - American Association of State Highway and Transportation Officials
date accessioned2017-09-04T16:58:22Z
date available2017-09-04T16:58:22Z
date copyright2014.01.01
date issued2014
identifier otherXIYLIFAAAAAAAAAA.pdf
identifier urihttps://yse.yabesh.ir/std/handle/yse/121735
description abstractThis method covers preparation of specimens and the measurement of the change of diametral tensile strength resulting from the effects of water saturation and accelerated water conditioning, with a freeze–thaw cycle, of compacted asphalt mixtures. The results may be used to predict longterm stripping susceptibility of the asphalt mixture and evaluate liquid antistripping additives that are added to the asphalt binder or pulverulent solids, such as hydrated lime or portland cement, which are added to the mineral aggregate. The values stated in SI units are to be regarded as the standard.
This standard may involve hazardous materials, operations, and equipment.
This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
languageEnglish
titleAASHTO T 283num
titleStandard Method of Test for Resistance of Compacted Asphalt Mixtures to Moisture-Induced Damageen
typestandard
page9
statusActive
treeAASHTO - American Association of State Highway and Transportation Officials:;2014