SAE AMS4941F
Titanium Tubing, Welded 40 ksi (276 MPa) Yield Strength - UNS R50400
Organization:
SAE - SAE International
Year: 2012
Abstract: Form
This specification covers one grade of commercially pure titanium in the form of welded tubing.
Application
This tubing has been used typically for parts, such as low-pressure fluid-conducting lines and conduits, requiring strength up to 400 °F (204 °C) and oxidation resistance up to 600 °F (316 °C), but usage is not limited to such applications.
This specification covers one grade of commercially pure titanium in the form of welded tubing.
Application
This tubing has been used typically for parts, such as low-pressure fluid-conducting lines and conduits, requiring strength up to 400 °F (204 °C) and oxidation resistance up to 600 °F (316 °C), but usage is not limited to such applications.
Collections
:
Show full item record
contributor author | SAE - SAE International | |
date accessioned | 2017-09-04T16:46:11Z | |
date available | 2017-09-04T16:46:11Z | |
date copyright | 04/01/2012 | |
date issued | 2012 | |
identifier other | WBRUUEAAAAAAAAAA.pdf | |
identifier uri | http://yse.yabesh.ir/std/handle/yse/109488 | |
description abstract | Form This specification covers one grade of commercially pure titanium in the form of welded tubing. Application This tubing has been used typically for parts, such as low-pressure fluid-conducting lines and conduits, requiring strength up to 400 °F (204 °C) and oxidation resistance up to 600 °F (316 °C), but usage is not limited to such applications. | |
language | English | |
title | SAE AMS4941F | num |
title | Titanium Tubing, Welded 40 ksi (276 MPa) Yield Strength - UNS R50400 | en |
type | standard | |
page | 8 | |
status | Active | |
tree | SAE - SAE International:;2012 | |
contenttype | fulltext |