AASHTO T 321
Standard Method of Test for Determining the Fatigue Life of Compacted Hot Mix Asphalt (HMA) Subjected to Repeated Flexural Bending
Year: 2011
Abstract: This standard provides procedures for determining the fatigue life and fatigue energy of 380 mm long by 50 mm thick by 63 mm wide hot mix asphalt (HMA) beam specimens sawed from laboratory or field compacted HMA and subjected to repeated flexural bending until failure.
This standard may involve hazardous materials, operations, and equipment. This standard does not purport to address all of the safety concerns associated with its use. It is the responsibility of the user of this procedure to establish appropriate safety and health practices and to determine the applicability of regulatory limitations prior to use.
This standard may involve hazardous materials, operations, and equipment. This standard does not purport to address all of the safety concerns associated with its use. It is the responsibility of the user of this procedure to establish appropriate safety and health practices and to determine the applicability of regulatory limitations prior to use.
Show full item record
| contributor author | AASHTO - American Association of State Highway and Transportation Officials | |
| date accessioned | 2017-09-04T16:02:03Z | |
| date available | 2017-09-04T16:02:03Z | |
| date copyright | 01/01/2007 (R 2011) | |
| date issued | 2011 | |
| identifier other | RMSXXEAAAAAAAAAA.pdf | |
| identifier uri | https://yse.yabesh.ir/std/handle/yse/65286 | |
| description abstract | This standard provides procedures for determining the fatigue life and fatigue energy of 380 mm long by 50 mm thick by 63 mm wide hot mix asphalt (HMA) beam specimens sawed from laboratory or field compacted HMA and subjected to repeated flexural bending until failure. This standard may involve hazardous materials, operations, and equipment. This standard does not purport to address all of the safety concerns associated with its use. It is the responsibility of the user of this procedure to establish appropriate safety and health practices and to determine the applicability of regulatory limitations prior to use. | |
| language | English | |
| title | AASHTO T 321 | num |
| title | Standard Method of Test for Determining the Fatigue Life of Compacted Hot Mix Asphalt (HMA) Subjected to Repeated Flexural Bending | en |
| type | standard | |
| page | 11 | |
| status | Active | |
| tree | AASHTO - American Association of State Highway and Transportation Officials:;2011 | |
| contenttype | fulltext |